Monday, September 28, 2009

[MW:3339] Re: Hydrotest flange thickness calculation

On Sun, Sep 27, 2009 at 10:25 PM, Arunachalam A <arunvani@gmail.com> wrote:
Use UG 34 of ASME Section VIII Div 1
 


 
On Sun, Sep 27, 2009 at 5:36 PM, Chaitanya Purohit <chaitanya_purohit@yahoo.co.in> wrote:
Dear Friends,

Please help to reply to the below query....

---------- Forwarded message ----------
From: Mithun Murali <Mithun.Murali@dodsaldxb.ae>
Date: 2009/9/27
Subject: Query regarding Hydrotest flanges
To: chaitanya_purohit@yahoo.co.in

Hi Chaitanya,

Can you ask this query in the group as I am unable to do so.

Any calculation sheet or method available for Thickness calculation for Blind Flange for 64 " CS pipeline hydrotest.(test pr of 83 barg), 400# rating.

I had referred to one of the Client spec, which demands 170mm thick plates for the same.

Any reference of Agency or Consultant doing these kind of Calculations.

 

Thanks and regards,

Mithun

Design Engineer - Piping

Dodsal Engineering & Construction Pte. Ltd.

Dubai, U.A.E.

Phone : +9714-3161279







--
ARUNACHALAM.A
050-5257122

Happiness Keeps You Sweet,
Trials Keep You Strong,
Sorrow Keeps You Human,
Failure Keeps You Humble &
Success Keeps You Glowing,
But Only Faith & Attitude Keeps You Going



--
ARUNACHALAM.A
050-5257122

Happiness Keeps You Sweet,
Trials Keep You Strong,
Sorrow Keeps You Human,
Failure Keeps You Humble &
Success Keeps You Glowing,
But Only Faith & Attitude Keeps You Going

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...