[MW:3314] RE: 3313] Filler wire for P45 to P8

You can use ER385/E385 (same used for P45) for P8 to P45 also

 

It is often used use in constructions of the ASTM 316 type, where a ferrite- free weld metal is required, e.g. in cryogenic or non-magnetic applications.

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of BHARAT GOLE
Sent: Friday, September 25, 2009 10:46 AM
To: Material Welding
Subject: [MW:3313] Filler wire for P45 to P8

 

Which is suitable filler wire for welding SS with SB 677 UNS N08904 i.e. P 8 to P45
Regards

Bharat B. Gole





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...