[MW:3086] RE: 3083] Re: Regarding the NDT to be carried out for 60 mm thick austenitic stainless steel plates

Dear friends ,

As per my suggestion, you better to select Co.60 only because the Ir -192 source is can do max .50 mm is sufficient but the code says can do upto 69mm .practically you can select the source Co -60 and you can save time as well as will achieve the sensitivity ,what the code and spec. recommended.

R.Ramu

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shashank Vagal
Sent: Sunday, August 30, 2009 1:21 PM
To: materials-welding@googlegroups.com
Subject: [MW:3083] Re: Regarding the NDT to be carried out for 60 mm thick austenitic stainless steel plates

 

Nilesh,
Why would you do these things?
1. No co60 for 69 mm SS?
2. High Strength and Low Strength Ir 192 are same in their pen power.
3. UT of 60 mm SS - well, can you please pass me the proc? I am curious. Twin crystal for what reasons?
Shashank Vagal

--- On Sun, 30/8/09, SENTHILKUMAR SWAMINATHAN <skumarswami@yahoo.co.in> wrote:


From: SENTHILKUMAR SWAMINATHAN <skumarswami@yahoo.co.in>
Subject: [MW:3082] Re: Regarding the NDT to be carried out for 60 mm thick austenitic stainless steel plates
To: materials-welding@googlegroups.com
Date: Sunday, 30 August, 2009, 2:44 PM

High Curie or Low Curie only helps in time factor. But Ir 192 Penetration is same from Low and High. If am wrong correct me.

 

S.Senthilkumar

--- On Sun, 30/8/09, Yadav Shiva <luvshiv2002@gmail.com> wrote:


From: Yadav Shiva <luvshiv2002@gmail.com>
Subject: [MW:3080] Re: Regarding the NDT to be carried out for 60 mm thick austenitic stainless steel plates
To: materials-welding@googlegroups.com
Date: Sunday, 30 August, 2009, 2:38 PM

hi,

           you can go for high strength - 192, but dont go for cobalt 60 since we use for thickness ranging more than 100 to  & 150 mm above.

On Sun, Aug 30, 2009 at 11:48 AM, Nilesh Pathare <patharenil@gmail.com> wrote:

Hi,
If your specification permits for RT or UT you can carry out any of these test for 60 mm Thick S.S.
For RT you may need cobalt 60 or High strength iridium 192.
For Ultrasonic Testing you shall use the RTD Twin crystal longitudinal wave Angle probes.

Regards,
Nilesh Pathare.

On Sun, Aug 30, 2009 at 10:35 AM, Stephen <stephenipr@gmail.com> wrote:


I wanted to know which NDT to be carried out for 60 mm thick
austenitic stainless steel plates welded using TIG welding




--
Best Regards,

Nilesh Pathare

 

 


start: 2008-06-21 end: 0000-00-00


Looking for local information? Find it on Yahoo! Local

 


See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---