If you use API 1104 Code, when the pipe is welded on the ground, the working clearence around ethe pipe at hte weld should not be less than 16 in. (4oo mm). When the pipe is welded in a trench, the bell hole enough to provide the welder or welders with ready access to the joint.
 
Regards
Ruscitto
  
>>> daniel iordache <daniel.iordache@gmail.com> 28/08/2009 04:18 am >>>

dear all,

i have 3 pipeline burried ...i need to know what minimum spacing is
recommanded....(api 1104/ b31.4)

thanks

regards

--
Daniel Iordache
Bureau Veritas - Angola
Mechanical Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
           daniel_iordache@yahoo.com

*********************************************************************

¡IMPORTANTE!

Para evitar accidentes por inhalación de monóxido de carbono:

- Mantenga los ambientes ventilados en forma permanente.

- Revise que la llama sea color azul y uniforme.

- Instale y haga revisar periódicamente sus artefactos sólo a través de gasistas matriculados.

Recuerde que los artefactos a gas pueden emitir Monóxido de Carbono: un gas altamente tóxico e imperceptible.

Más consejos en http://www.metrogas.com.ar

*********************************************************************

Este mensaje es privado y confidencial y va dirigido sólo al destinatario indicado. Si lo ha recibido por error, por favor avísenos inmediatamente vía e-mail a error-mail@metrogas.com.ar y tenga la amabilidad de eliminarlo de su sistema. La utilización o divulgación de su contenido puede importar la comisión de un delito. No copie, reproduzca o divulgue -en forma parcial o total- su contenido. Cualquier opinión contenida, es exclusiva de su autor y no representa la opinión de MetroGAS S.A. - Muchas gracias.

This message is private and confidential and it is only intended for the addressee named above. If you have received this message and it is not addressed to you, please advise us immediately at error-mail@metrogas.com.ar and kindly remove it from your system. The use or disclosure of its contents may be regarded as an offense. Do not copy, reproduce or disclose them, either partially or fully. Opinions are the exclusive responsibility of the author and do not represent the opinion of MetroGAS S.A. - Thank you.

:: http://www.metrogas.com.ar

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...