Dear Prashant ,
 
Need to Qualify the PQR as per AWS D 1:1 in 6GR position for the TKY joint and to confirm it covers your max. and min Dihedral direction plus the mock up pieces .
 
You ned to conduct the Mock up pieces which will cover your Dihedral angle as covered in 4.12.4 section of AWs D 1:1 .
 
Let me know if any more details are required ,
 
Regards,
 
sujeet Sangle

 
On Wed, Aug 26, 2009 at 11:17 PM, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
Dear all.
I' ve to fabricate platform as per API RP 2A.
Shall I qualify 6GR for T,K,Y joints? or shall I go for min & max. dihedral angle & min & max. root gap qualification.
psp  


Love Cricket? Check out live scores, photos, video highlights and more. Click here --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...