Thursday, August 27, 2009

[MW:3032] Re: 3018] p no

Dear all
is it correct that for steels that has a specification another of asme II find equivalent steel,P no ?
regards.

On Wed, Aug 26, 2009 at 9:26 AM, Muhammad Ijaz <m_ijaz@ffc.com.pk> wrote:

Dear Mano,

 

As per Stahlschluseel 2007, G4859 is equivalent to A351 (CT15C). So the corresponding P no. shall be P. no. 45 as per ASME IX 2007.

 

Regards,

Muhammad Ijaz


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Manoharan Kalimuthu
Sent: Tuesday, August 25, 2009 9:56 PM
To: materials-welding@googlegroups.com
Subject: [MW:3018] p no

 

Dear all

We have material G4859 (its in the ISO) I would like to know what is the P NO for this ....

Regards

Mano






--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...