[MW:2833] Toughness Requirement for Dissimilar Weld

Your understanding is correct. It is exempted


From: Vivek Bhisade [mailto:vivek@tpr.grengg.com]
Sent: Tuesday, July 28, 2009 2:20 PM
To: materials-welding@googlegroups.com
Subject: Toughness Requirement for Dissimiller Weld

 

 

Dear All,

 

We have a  job ( hydro generator) material SA 387 Gr.11 CL 2 + SS347 ( clad) ,required impact testing at (minus)-18 Deg.C with energy value 33 J average (irrespective of MDMT ),having some nozzles (LWNR) material is SA 182 F 347.   

For  Welding Procedure Qualification of Dissimilar metals Nozzle to Shell joint ( P4 To P8) using electrodes by E309L , weld Impact test is required or not?

As per ASME SEC VIII Div 1 – UHA-51 (e) it is exempted ,

Please advise.

 

Thanks in advance.

 

 

 

 

 

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...