Friday, July 24, 2009

[MW:2805] Inconel 600


Hi Guys,
 
Please tell me what is the best match of the filer material and gas for welding ALLOY 600 ( plates 1/4"up to3/") using MIG and TIG procedures.
If you also have some welding giudelines - welding procedure regardless, it will be great
Getting an answer ASAP it will be very much apreciated
 
Thanks a lot
Sorin St.




Stay on top of things, check email from other accounts! Check it out.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...