Friday, July 24, 2009

[MW:2796] RE: 2789] Additional Welding layers

No of passes doesn’t matter, as long as your T and t limits are within the boundary.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohamed Mubarak Syed
Sent: Thursday, July 23, 2009 6:32 PM
To: materials-welding@googlegroups.com
Subject: [MW:2789] Additional Welding layers

 

Can any one clarify,

 

We have appproved WPS Which is showing  8 passes, to cover the thickness of PQR apecimen (12.7 mm), But thickness range is 6.9mm to 19.1mm, We have production welding thickness is 18 mm,

 

So we need to do additional weld passes to cover the required thickness, approximately 12 passes in production welding

 

Kindly advice



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...