[MW:2595] Re: Welding Ti tube to Ni-Al-Bronze weld overlay

Expand only with grooves, no welding tube-to-tubesheet.

Regards,

T. Rizal H

On Tue, Jun 30, 2009 at 11:45 AM, Raghuram
Bathula<raghurambathula@gmail.com> wrote:
>
> I have come across a HE data sheet specifies Ni-Al-Bronze weldoverlay
> on CS tubesheet and tubes as Titanium. How these will be joined any
> idea, please advice?
>
> >
>

--
Regards,

T. Rizal Hidayat

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...