I writing WPS that will include a Temperbead Tech, Preparing a set to
test WPS at the shop Facilities using
28 inch runpipe with 6 to 8 inch brach. What kind of mechanical tesing
shall be expected, if the code of construction will be ASME Sec.8 Div
1?
i know there will be a hardness test, any other help some pne can give
me idea to test?