Thursday, June 25, 2009

[MW:2545] Re: Does any body knows about water tight weld.

It is the same as seal weld and ASME IX have special conditions for that weld type.

Regards

Fernando Gameiro

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of harish katesia
Sent: quinta-feira, 25 de Junho de 2009 11:22
To: materials-welding@googlegroups.com
Subject: [MW:2543] Does any body knows about water tight weld.

 


Dear all,

 

Can anybody tell me what is water-tight weld & how to ensure this.

 

Do we have any standards for this or does ASME talks for this.?


--
Regards,
Harish katesia
Mob no.09601551774



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...