fill with water, if it doesn't leak its water tight!!
ASME has requirements for hydro test depends on design conditions and the applicable code. 

It is necessary to specify the type of item and applicable code, design conditions etc, to have appropriate answer.


On Thu, Jun 25, 2009 at 2:21 PM, harish katesia <harish.katesia@gmail.com> wrote:

Dear all,
 
Can anybody tell me what is water-tight weld & how to ensure this.
 
Do we have any standards for this or does ASME talks for this.?

--
Regards,
Harish katesia
Mob no.09601551774





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...