Dear Monica,
 
You can use TIG (GTAW) or MIG (GMAW) methode and filler metal with AWS code ERCu
C7(Copper filler metal, tin-alloyed with good flow properties),
gas: Argon-Helium, preheat to exclude discontiniuties..
 
regards,
 
Arjan 
 
> Date: Wed, 24 Jun 2009 07:11:36 -0700
> Subject: [MW:2529] copper
> From: raphaelriccio@gmail.com
> To: materials-welding@googlegroups.com
>
>
> Hi,
>
> I have a big copper statue (monument) that i need to repair. which is
> the best welding?
>
> thanks,
> monica
>
> --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...