Monday, June 22, 2009

[MW:2508] Re: BACK WELD

Welding qualification w/o BW allows backwelding on the job; but not vice versa. You have to requalify using BW.

--- On Sun, 14/6/09, Ali Asghari <asghariali@rocketmail.com> wrote:

From: Ali Asghari <asghariali@rocketmail.com>
Subject: [MW:2429] BACK WELD
To: materials-welding@googlegroups.com
Date: Sunday, 14 June, 2009, 11:47 AM

HI
 in DNV-OS-F101(APPENDIX C),BACK WELD (DELETION OR ADDITION )IN ESSENTIAL VARIABLES NOT NOTED.
IN PRODUCTION A PROBLEM OCCURED THAT MUST BE BACK WELDED.
NOW THIS IS ALLOWED OR NOT?(WELDING QUALIFICATION DOESN'T HAVE BACK WELD)
RJD





ICC World Twenty20 England '09 exclusively on YAHOO! CRICKET --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---