Wednesday, May 27, 2009

[MW:2242] Re: 2238] pump damage

Nilesh,
Thanks a lot for this splendid artcle. Very useful for all in the field. Appreciate.
Regards,
Shashank Vagal


--- On Wed, 27/5/09, Darji Nilesh (Mumbai - Machinery) <N.Darji@ticb.com> wrote:

From: Darji Nilesh (Mumbai - Machinery) <N.Darji@ticb..com>
Subject: [MW:2239] RE: 2238] pump damage
To: materials-welding@googlegroups.com
Date: Wednesday, 27 May, 2009, 10:01 AM

Sadique,

Refer attached article. For Nanhai we used Gaussmeter to check residual
magnetic field in Pumps as Client observed that during Pump
suction/discharge pipe welding, Flanges were bolted to pump flanges.

With regards,

Nilesh Darji
Engg. & Designs Tecnimont ICB
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Sadique Sheikh
Sent: Tuesday, May 26, 2009 7:48 PM
To: materials-welding@googlegroups.com
Subject: [MW:2238] pump damage


Hello all of you.
I have one query and may hope the answer from expert member from field.
On our site,the welder did the welding of pipe while the pipe flange
was bolted to pump.so that time small spark occured between the flange
and the noise enclosure i.e cover of pump as some paint removed from
edge of enclosure which was in direct contact with flange that time.
So my question is can it affect the bearing of pump as pump base is
already grounded.
Regards
Sadique





Filtered by Hosted Filtering



Bring your gang together. Do your thing. Find your favourite Yahoo! Group. --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...