Dear Saqib,

Firstly do not use word "SAND" Blasting as most of the countries it is prohibited.

Next to your query, Yes before doing insulation some surface cleaning might be necessary. Depends on the customer specification and type of insulation and environment(site condition) one can make decision whether to carry out blasting or not.

Basically blasting is required for developing profile on the substrate (steel surface) and if the insulation method where you do not need profiled surface you can replace blasting with power tool cleaning (hand tool cleaning if area is not big).

It is always better to remove mill scale and any detrimental chemicals prior to carry out insulation to prevent oxidation / corrosion under the insulation.

C. K. Purohit


--- On Mon, 18/5/09, saqib gul <saqibgul@gmail.com> wrote:

From: saqib gul <saqibgul@gmail.com>
Subject: [MW:2197] Re: 2195] Re: Sand blasting
To: materials-welding@googlegroups.com
Date: Monday, 18 May, 2009, 11:13 AM

Before insulation cleaning of pipe lines by sand blasting is required or not?
 
Mr. Singh: No? but why?
Is there no need for cleaning the pipe lines even manually (by power brush etc.)?

On Mon, May 18, 2009 at 10:30 AM, Nachhattar Singh <n.singh@moodyint.com> wrote:

The straight answer to the question is   NO




Nachhattar Singh
Director


Telephone: 91-22-2758 0044 91-98201 81158
Fax: 91-22-27580033
Email: n.singh@moodyint.com
Web http://www.moodyint.com/

Moody International (I) Pvt Ltd 32 / 33 Gautam Complex , Sector - 11
C.B.D Belapur , Navi Mumbai - 400 614
Maharashtra (India)  Mumbai Maharashtra 400 614 India




 Moody Group Confidentiality Note: The information transmitted is intended only for the person(s) or entity to which it is addressed. It may contain confidential and/or privileged information or material. Any review, retransmission, dissemination to other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and delete the material from any computer.

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of BR
Sent: Monday, May 18, 2009 10:58 AM
To: Materials & Welding
Subject: [MW:2195] Re: Sand blasting


Why you want to balst the insulation? be more clear on querry pl.?

On May 18, 8:54 am, Saqib <saqib...@gmail.com> wrote:
> Is it recommended to sand blast the Insulated pipe lines?
>
> Regards
> Saqib














Share files, take polls, and make new friends - all under one roof. Click here. --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...