[MW:1850] Re: 1841] Re: 1838] Fabricated Stiffeners

Its so because the design is guided by buckling and not induced stress.


Inactive hide details for "Somesh Kumar Pandey" <Somesh.Kumar@kbr.com>"Somesh Kumar Pandey" <Somesh.Kumar@kbr.com>


          "Somesh Kumar Pandey" <Somesh.Kumar@kbr.com>
          Sent by: materials-welding@googlegroups.com

          03/30/2009 11:58 AM

          Please respond to
          materials-welding@googlegroups.com

To

<materials-welding@googlegroups.com>

cc


Subject

[MW:1843] RE: 1841] Re: 1838] Fabricated Stiffeners


Devang,

As per ASME it is no where specified for external pressure design to use
the staggered intermittent weld to fabricate the stiffeners. Hence, in
my opinion it should not be used. You have to meet the required moment
of inertia for the provided section. It is advisable to fabricate the
stiffener with continuous welding only.

Regards

Somesh Kumar Pandey
KBR Energy & Chemicals
79 Anson Road #20-01
Singapore 079906
Office: +65 6210 7459
Fax: +65 6210 7250
Email: Somesh.Kumar@kbr.com


-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Devang Patel
Sent: March 30, 2009 1:48 PM
To: materials-welding@googlegroups.com
Subject: [MW:1841] Re: 1838] Fabricated Stiffeners


Thanks, Somesh,

Yes, you are write but my question is can we do staggered intermittent
weld
to fabricate the stiffeners?

ASME Sec. VIII Div-1 told about the stiffeners to shell welding only.


Regards,


Devang Patel
Manager Engineering

INOX INDIA Ltd.
Ph :+91-265-3056392-3056100
Fax :+91-265-2333398-2341449
email : devangp@inoxindia.com
www.inoxindia.com

----- Original Message -----
From: "Somesh Kumar Pandey" <Somesh.Kumar@kbr.com>
To: <materials-welding@googlegroups.com>
Sent: Monday, March 30, 2009 10:45 AM
Subject: [MW:1840] RE: 1838] Fabricated Stiffeners



Dear Devang,

Fabricated stiffeners can be used in external pressure design of shell
of
pressure vessel as per ASME Sec. VIII Div.1. You can refer UG -29 , Fig.
UG 29.1 , UG-30 & Fig. UG-30 of ASME Sec. VIII Div.1 for more details on
the acceptable method of attaching stiffener rings

Regards

Somesh Kumar Pandey
KBR Energy & Chemicals
79 Anson Road #20-01
Singapore 079906
Office: +65 6210 7459
Fax: +65 6210 7250
Email: Somesh.Kumar@kbr.com

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Devang Patel
Sent: March 30, 2009 12:24 PM
To: materials-welding@googlegroups.com
Subject: [MW:1838] Fabricated Stiffeners


can we use fabricated stiffeners in external pressure design of shell of

pressure vessel?

If, yes than please tell, can we use staggered intermittent weld to
fabricate T or Angle?

Please reply.


Regards,


Devang Patel
Manager Engineering

INOX INDIA Ltd.
Ph :+91-265-3056392-3056100
Fax :+91-265-2333398-2341449
email : devangp@inoxindia.com
www.inoxindia.com



This e-mail, including any attached files, may contain confidential and
privileged information for the sole use of the intended recipient.  Any
review, use, distribution, or disclosure by others is strictly
prohibited.
If you are not the intended recipient (or authorized to receive
information
for the intended recipient), please contact the sender by reply e-mail
and
delete all copies of this message.









--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...