[MW:1795] Re: Polarity Vs Heat generation

+ve side heat will be more . 
Tagore 

On Sun, Mar 22, 2009 at 2:38 PM, Tirumala B N Tagore <tagore.tbn@gmail.com> wrote:


On Sun, Mar 22, 2009 at 9:22 AM, Muhammed Ibrahim <ibratech@gmail.com> wrote:

Hi members,
 
I would like to get a clarification in a matter. Is there any recomendation to use electrode -ve for overlay to get less dilution?. Is there any relation with electrode polarity and heat generation?.

Thanks & Regards
Muhammed Ibrahim PK





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...