Tuesday, March 17, 2009

[MW:1770] Re: 1764] Hot Induction Bend

I agree with Francis , and if you want to cut the hot bend , cut from end at stright protion only. and remmber atleast left the stright  length 0.7 x d ( dia of pipe ) min with pipe after cutting of bend.
 
after cutting , edge shd be check with UT up too 100 mm both side and for teh surface checking go for the MT.
 
Regards
 
Rajeev
 


 
2009/3/16 <francis.lobo@indiatimes.com>

Dear All,
Hot Bends can be cut by cold cutting or gas cutting as normal piping in carbon steel, but you need to be more worried on dimensional problems as the ovality issue will come into picture thereby you may land into bad fit up problems and also some time pigging issues as standard allows the more tolerances on body and tighter tolerances on both ends and reduced wall thickness on body of a bend.

If any impact testing requirements are involved weld procedure may be qualified accordingly to ensure the properties.

Pl check the ovallity, thickness and lamination by UT, MPI of new beveled edges and also gauging prior to any fit up.

Refer Bend standards ASME B 16.49 and TPA -IBS -98

Best Regards,
Francis Lobo

----- Original Message -----
From: Ravi Yeleswarapu <ravi.yeleswarapu@c-a-m.com>
To: materials-welding@googlegroups.com
Sent: Mon, 16 Mar 2009 09:41:18 +0530 (IST)
Subject: [MW:1765] RE: 1764] Hot Induction Bend


Hi VJV,
Cold cutting is always preferable than hot or gas cutting, as cold
cutting will not alter metallurgical properties.
One of other things to be considered is profile to suit the ID/OD of the
joining pipe/fitting.

Ravi

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of VJ V
Sent: Sunday, March 15, 2009 5:30 PM
To: Materials & Welding
Subject: [MW:1764] Hot Induction Bend


Hi All,

Is there any technical adversity in Cold cutting a Hot induction Bend
( Hot formed at around 860 Deg C and then Stress relieved) to suite to
site condition ? I think Hot work-oxy aceteline cutting etc- is not
acceptable...

But Can the Hot Induction Bend be undergone cold cutting...
other than Metallurgical consequence any thing else to be considered
while cold cutting ?

Thanks
VJV


~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

This email message is for the sole use of the intended
recipient(s) and may contain confidential and privileged
information of Cameron and its Operating Divisions.
Any unauthorized use or disclosure is prohibited.
If you are not the intended recipient, please contact the
sender by reply email and delete and destroy all copies
of the original message inclusive of any attachments.

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~





--
Exclusive spy camera shots of the Tata Nano only on ZigWheels.com
http://www.zigwheels.com/tata-nano/

WHEN YOU ARE JUST AN OPTION FOR THEM....."

SO , Always keep in mind that......

DON'T GO THE WAY LIFE TAKES YOU,
TAKE THE LIFE THE WAY YOU GO,

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...