the nominal thickness of the pipe is the thickness ordered by client or design thickness on which the tolerances as per api 5l is applied tolerance are different for different nominal thickness as per new api 5l
 Dinesh verma
On Fri, 27 Feb 2009 22:04:19 +0530 materials-welding@googlegroups.com wrote
Hi Mr. Babu,
 
Nrmally Nominal thickness is the thickness which we can take w.r.t schedule wheras the actual thickness can be +/- 12.5% of the nominal thickness.
 
Mukesh
Lurgi

On Sat, Feb 14, 2009 at 9:49 PM, babu k wrote:


Hi,
 
Let me introduce my self, I am Babu Working in Singapore.
 
I would like to '' What is the Physical Meaning of Nominal thickness''  which is referred in all API codes and How it is differ from the Actual thickness,
 
Thanks & Regards,
 
K.Babu
 











--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...

Shopping

Pages

Contributors

Blog Archive