Thursday, February 26, 2009

[MW:1658] Re: Difference between Full & 100 % radiography

So far as I know the Full Radiography is the term used for PV fabrication.
It is defined in ASME sec.VIII/UW-11. It is not 100% radiography as some of
the joints are excluded from the requirement of RT (for e.g. nozzle butt
welds with DN 250 and smaller that are thinner than 29 mm)

On the other hand, 100% Radiography is the term used in piping fabrication.
And it implies 100% radiography of all the butt joints.

But some times Client may ask 100% RT in PV also.

Hope it clarifies.

Best regards,

Prasad



Sudipto_Banerjee@
fwuk.fwc.com
Sent by: To
materials-welding materials-welding@googlegroups.com
@googlegroups.com cc

Subject
26/02/09 04:41 PM [MW:1654] Difference between Full &
100 % radiography

Please respond to
materials-welding
@googlegroups.com

I want to know the Difference between Full & 100 % radiography and the
code/cases that is being spelt out.

Thanks.


Best Regards,
Sudipto Banerjee


This email and the information it contains:-
(a) is intended for the person(s) or organisation(s) named above and for no
other person(s) or organisation(s); and
(b) may be confidential, legally privileged and protected in law.
Unauthorised use, copying or disclosure of any of it may be unlawful.

If you have received this email in error, please contact the sender
immediately at his/ her email address or at Postmaster@fwuk.fwc.com and
delete this email and any attachments.

Please note that any views or opinions in this email are those of the
author and do not necessarily represent those of Foster Wheeler Energy
Limited or any of its associated companies.

Unless otherwise stated, neither this email nor any attachments constitute
an offer and nor are they intended to create a contractual relationship or
be contractually binding.

This email has been generated through the email systems of Foster Wheeler
Energy Limited although the email may in fact be from an associated company
of Foster Wheeler Energy Limited or an individual. Should you require
further details about the entity or individual on behalf of which this
email is sent, please contact the sender or Postmaster@fwuk.fwc.com.

Foster Wheeler Energy Limited
Shinfield Park
Shinfield
Reading
Berkshire
RG2 9FW
UK

A company registered in England and Wales No:1361134

Tel: +44 (0)118 913 1234
Fax:+44 (0)118 913 2333

Save a tree...please don't print this e-mail unless you really need to.


Save a tree...please don't print this e-mail unless you really need to.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments: