Wednesday, February 25, 2009

[MW:1621] RE: 1620] PIPE SA106GRB

Dear Srinivasan,

 

It’s a good question but I will prefer you to find the answer yourself. It is given in the code section 2A (SA 106) and ASTM A106 too….

 

Regards.

 

C. K. Purohit

General Manager - QC

KNM Process Systems Sdn Bhd - Malaysia

 

HP No. : 6016-3376448


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Srinivasan R.
Sent: Wednesday, February 25, 2009 2:16 PM
To: materials-welding@googlegroups.com
Subject: [MW:1620] PIPE SA106GRB

 

Why SA106GRB  pipe is available only as  seamless pipe and not welded.

 

Regards ,

 

Srinivasan.R

Piping Dept.

 






***DISCLAIMER NOTICE ***

"This email and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above. If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited. If you receive this email in error, please notify the sender immediately by return email and delete the email and any of its attachments. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...