Dear Mr. Jivan Dhamane,

 

As per ASME B31.3 Pneumatic test of RF pad is not mandatory, if there is any defect in RF Pad weld, during hydrotest of the main line you can find out because of the Hydrostatic pressure in main line.

 

With regards,

 

S. SIVASUBRAMANIAN

QA/QC Manager

Larsen & Toubro Kuwait Construction Company

P.O. Box.1082, Fintas 51011, KUWAIT

Mobile: 00965 66387188, 00965 94005327

Fax: 00965 66321511


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ramprasad Chari
Sent: Thursday, February 19, 2009 6:55 AM
To: materials-welding@googlegroups.com
Subject: [MW:1599] Re: Pneumatic test of Reinforcement Pad for Branch connection in Piping

 

Irrespective of, whether it is mentioned in code or not RF pad has to be pneumatically tested otherwise how will you check leakage in "welds" associated with RF pad.

Regards

Aarpee

On Wed, Feb 18, 2009 at 10:07 PM, Jivan Dhamane <jivanadhamane@yahoo.co.in> wrote:

Dear Friends

 

I would like to know whether Pneumatic Test of Reinforcement Pad for branch connection of Process Piping is mandatory as per ASME B31.3. I searhed but I could not found any paragraph in ASME B31.3.

 

Regards

 

Jivan Dhamane

 


Cricket on your mind? Visit the ultimate cricket website. Enter now!




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...