[MW:1596] Fw: Mix up of A106 Gr.B and A336 Gr.6 pipes

Friends,
 
Sorry for the typographical error.
 
Please read A336 Gr.6 as A333 Gr.6.
Any non-destrictive test method that can sagregate the mixed material.
 
Regards,


T S Reddy
Mobile: 919998215568
India


----- Forwarded Message ----
From: tamma reddy <tsr_52@yahoo.co.in>
To: materials-welding@googlegroups.com
Sent: Sunday, 15 February, 2009 4:25:06 PM
Subject: Mix up of A106 Gr.B and A336 Gr.6 pipes

Dear Friends,
 
When A106 Gr.B and A336 Gr.6 pipes are physically mixed up and mill identification/ stencilling was lost during painting on external surface. Since both are CS materials, segregation by PMI (i.e by X-Ray spectrometer or by Gamma ray) is not possible..
 
Is there any other NDE method to segregate/ identify them to the respective material specification.
 
Regards,
T S Reddy



Add more friends to your messenger and enjoy! Invite them now.


Add more friends to your messenger and enjoy! Invite them now.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...