[MW:1588] Re: Mix up of A106 Gr.B and A336 Gr.6 pipes

Dear Mr. Reddy,
 
the mechanical properties of the two steel grades differ, significantly . It might be worth a try to distinguish between them using portable hardness testing like Equotip or Krautkrämer.
 
Best of luck,
Tjitte Schutter
 
ILF Consulting Engineers
Munich, Germany


 
2009/2/15 tamma reddy <tsr_52@yahoo.co.in>
Dear Friends,
 
When A106 Gr.B and A336 Gr.6 pipes are physically mixed up and mill identification/ stencilling was lost during painting on external surface. Since both are CS materials, segregation by PMI (i.e by X-Ray spectrometer or by Gamma ray) is not possible.
 
Is there any other NDE method to segregate/ identify them to the respective material specification.
 
Regards,
T S Reddy



Add more friends to your messenger and enjoy! Invite them now. --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...