Saturday, January 31, 2009

[MW:1484] RE: 1482] ASME VIII

Kim,

You can refer ASME Sec. VIII Div. 1 Cl. UG-115 through UG-120 for U
Stamp marking and report/ certificate requirement. For Pressure Relief
device you can get the requirements per Cl. UG-125 through UG-137 of
ASME Sec. VIII Div.1.

Regards

Somesh

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Kim
Sent: January 30, 2009 5:33 PM
To: Materials & Welding
Cc: shihyuen81@yahoo.com
Subject: [MW:1482] ASME VIII


Dear Sirs,

I am looking for the information about ASME VIII for the pressure
vassel, pulsation dampener & Pressure relief valve. Is ASME VIII have
any relation with 'U' Stamp? Does ASME VIII provide any coding /
certificate?

Thank's in advance.

Best Regards,
Kim


This e-mail, including any attached files, may contain confidential and privileged information for the sole use of the intended recipient. Any review, use, distribution, or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive information for the intended recipient), please contact the sender by reply e-mail and delete all copies of this message.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...