[MW:1481] RE: 1480] RE: 1479] CHLORINE INSTITUTE PAMPHLET 6 CLASS II - Requirement

Pamphlet 6: Piping Systems for Dry Chlorine
Edition 15, May 2005
Contains information on selected pipe, valves and fittings suitable for use with dry chlorine (gas or liquid).

In this new edition, CI incorporates vital lessons learned based on the investigation of the 2001 chlorine release in Festus, Missouri. Specifically, the Institute:

And also developed a new Appendix B Chlorine Service Fluid Category to document the position of the Chlorine Institute on the criteria outlined for Category M in ASME B31.3 as it impacts chlorine piping systems.

can be brought from http://www.chlorineinstitute.org/Bookstore/ProductDetail.cfm?ItemNumber=2258
or www.techstreet.com and it covers from design to layout, installation
For e.g. Appendix A, B. Installation & Maintenance
Section 10: Piping Lay out Design Considerations
Class II is applicable for the below condition
Gas only vacuum to 150 psig (1034 kPa) and -50°F to 300°F (-46°C to 149°C)

And Pamphlet 95 covers Gaskets for Chlorine Service (attached), also attached a valve catalogue used for cl service


-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Rajak, Sanjib (Bantrel Constructors)
Sent: Friday, January 30, 2009 10:20 AM
To: materials-welding@googlegroups.com
Cc: piping_valves@yahoogroups.com
Subject: [MW:1480] RE: 1479] CHLORINE INSTITUTE PAMPHLET 6 CLASS II - Requirement

FYI

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Kadam Vijay S.
Sent: January 29, 2009 10:53 AM
To: materials-welding@googlegroups.com
Cc: piping_valves@yahoogroups.com
Subject: [MW:1479] CHLORINE INSTITUTE PAMPHLET 6 CLASS II - Requirement

Dear All,

I have one piping class in LTCS material which is to be used for
CHLORINE GAS service.
With Design condition as follows:
Min 1.84 MPag@ -39 degC
Max 1.38 MPag@ 200 degC
Rating : 150#

For this class our Licensor along with code ASME B31.3 has given
requirement of CHLORINE INSTITUTE PAMPHLET 6 CLASS II.
Dear members can you explain me what exactly is this requirement, and if
its applicable only for valves or also for other fittings.
Thank You & Kind Regards
Vijay Kadam

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...