Friday, September 19, 2008

[MW:1151] FCAW --- UT / RT ???

 
Dear Friends

We are presently using FCAW process(E71T-1) for welding SA516Gr.70 material in 3G and 1G. The joint calls for 100% RT and UT. The thickness is 70mm with double V.
But everytime we get repair in the weld like slag, LOF,porosities..

So my basic question is can FCAW be used to weld RT and UT joints??
If yes what is the correct procedure / precautions to be followed..

Regards

Prem Nautiyal

PREM S NAUTIYAL
CELL : 9820313278

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...

Ebay

Pages

Contributors

Blog Archive