95 degree celcius minimum
 


 
2008/1/8 Vivek <vivek@tpr.grengg.com>
Hi, 
As we have a plate material SA 537 CL1 (45mm thk) with max.carbon equivalent 0.45 %, as per clients specification requirement (CE < 0.42%) ,we shall get the hardness <200 BHN & impact at           (minus)-47 Deg.C ( 27J Avg.) on WELD and HAZ after PWHT.
Kindly suggest us preheating temprature inorder to get above property.
 
vivek





--
Thanks & Regards
Muhammed Ibrahim PK


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...