[MW:970] Consumable For UNS31254 weldoverlay on SA516 Gr. 70

Has anybody experienced UNS31254 (P No. 8 Gr. 4.....chemi..20Cr 18Ni
6Mo) weldoverlay on SA516 Gr. 70
Can someone suggest the correct AWS class? If u can suggest the STRIP
consumable supplier for the smae it will be handful....