dear sir
i am a welding engg student and doing project on hydrogen cracking
of cr-mo steel by using implant test method.
the following result were observed

electrode diff hydrogen
level critical stress

E6013 (ruttile type) 5
ml 456 mpa
E9015 B9
10.6ml 500 mpa
according to theory if hydrogen level increases critical cracking
stress will decreases but in my exp critical cracking stress is coming
more in low level of hydrogen

i would like to have your comment on this result

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...