Tuesday, April 29, 2008

[MW:757] Material for 1'' BE Fittings

Hi Gents,

 

This is for 1'' fittings like Elbows, TEE etc

 

Appreciate if somebody could advice me whether I can accept this. The vendor is telling that if it's BE, then it will be A234 GR.WPB, SCH 160, BE for 1'' fittings.

 

Kindly advice.

 

As per Spec

Vendor offered

6000 LB, FS, BE A-181 GR.1

A234 GR.WPB, SCH 160, BE

6000 LB, FS, BE A-181 GR.1

A234 GR.WPB, SCH 160, BE

3000 LB, FS, BE A-181 GR.1

A234 GR.WPB, SCH 160, BE

 

 

Thank you,

 

Regards,

 

Sabir


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...