Evidently, if a kilogram sits around doing nothing for too long, it begins to lose weight. Or rather, mass. The 118-year-old cylinder that is the international standard for the metric mass, kept tightly under lock and key outside
Made of a platinum-iridium alloy, the cylinder was cast in 1889 and measures 1.54 inches in height and diameter. Of course, it has lost mass only in relation to the 80 or so reference kilograms that exist around the world. It could be that, locked away as it's been for over a hundred years, it has remained the same and the others have gained weight.
Click here for more information.
Thursday, September 20, 2007
When is a Kilogram Not a Kilogram?
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment