Tuesday, March 14, 2017

Re: [MW:26204] WPS reference on PQR-

Dear Sir,

I believe if the PQR was conducted followed by a Client approved pWPS, the WPS number might be indicated.

Regards
P Govindan

On Mar 14, 2017 06:40, "Kannayeram Gnanapandithan" <kgpandithan@gmail.com> wrote:
ASME SECTION IX,
QW-200.1
                   The WPS shall  reference the supporting Procedure Qualification Record
QW-200.2
                 The completed PQR shall document all Essential and whenrequired supplementary essential variables

     Nowhere it is mentioned that PQR shall reference the WPS
But some client?Auditors insists to mention the WPS no on PQR,  Why, when Code does not address it??
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNUAgjWQa0WVPPoxPZ1%2BDg94yEdEOd%2BfJWsCtgNW2%2BVzA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9eUpUVU1-mipAVdwbZ5DQEMsBhrx8p7MsfHMkYrunYxLw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...