Tuesday, March 14, 2017

Re: [MW:26203] WPS reference on PQR-

preliminary welding procedures are written for providing specific information to all during qualification. It is not necessary to indicate the pWPS/WPS numbers on the PQR. 
we can write 'n' number of WPS's supporting one PQR. do we write all of these WPS numbers on PQR?
refer interpretation # IX-10-22

On 14 March 2017 at 07:36, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
ASME SECTION IX,
QW-200.1
                   The WPS shall  reference the supporting Procedure Qualification Record
QW-200.2
                 The completed PQR shall document all Essential and whenrequired supplementary essential variables

     Nowhere it is mentioned that PQR shall reference the WPS
But some client?Auditors insists to mention the WPS no on PQR,  Why, when Code does not address it??
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

-

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubkVAgKUk5TcqYdDaHDtgoD0O-vsMfJZMET6SWrHUQiG7w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...