Sunday, March 12, 2017

Re: [MW:26195] as per ASTM E23 what is the minimum maximum thickness for impact test specimen?

Hi
Refer to Annex A3 for more sizes

Regards

On Sun, Mar 12, 2017 at 10:38 AM, sukumar <r.sukumech@gmail.com> wrote:
Sukumar
QA/QC engineer,
Saudi arabia.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d0af6bb8-8911-4489-ae8f-e53a45167457%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ASNT NDT Level III
International Welding Engineer

Mob.:+98 912 1394023




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtv7mr9Sa0brB3cYGFXxxS9c%2BUra2fFr7xTb-dqkgmKcag%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...