Re: [MW:26174] Fwd: Welder qualification test piece - examination length

if it for ASMEBPV IX, read, QW 302.2: the minimum length of coupon(s) to be examined shall be 6 in. (150 mm) and shall include the entire weld circumference for pipe(s), except that for small diameter pipe, multiple coupons of the same diameter pipe may be required, but the  number need not exceed four consecutively made test coupons. 
---------- Forwarded message ----------
From: chiluka venkatramulu <ramuluchiluka@gmail.com>
Date: Thu, Mar 9, 2017 at 4:54 PM
Subject: Welder qualifications
To: materials-welding <materials-welding@googlegroup.com>


Dear all,
When we qualify welder for performance qualification by NDT we need to take RT-150mm. My quarry is, if we need to qualify 1/2" pipe for diameter qualification, whether we need to weld 3 piece to take RT of 150mm.


Ragards,
Venkatramulu
 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3Da3jW8OD2ghfb8FCXs5WQ2cUc92T5ms12Ys59u-%3Dam6w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...