[MW:26202] WPS reference on PQR-

ASME SECTION IX,
QW-200.1
                   The WPS shall  reference the supporting Procedure Qualification Record
QW-200.2
                 The completed PQR shall document all Essential and whenrequired supplementary essential variables

     Nowhere it is mentioned that PQR shall reference the WPS
But some client?Auditors insists to mention the WPS no on PQR,  Why, when Code does not address it??
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNUAgjWQa0WVPPoxPZ1%2BDg94yEdEOd%2BfJWsCtgNW2%2BVzA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...