Wednesday, March 8, 2017

[MW:26159] Requirement of Heat Treatment on Pipe Specimen after Flattering Prior to Tensile test

Dear Experts,

Kindly advice,  According to SA 370 is it required Heat Treatment on Pipe Specimen after Flattering Prior to Tensile test as per below clause.





(PRASAHANT BARGE)
QA/QC Engineer
Cell:09967324773

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN7Vqcc4jR%2BzTp1PvpL6kVitOOqXDn-1PjEoBAmN3tf-_B1dMw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...