If it is in a jurisdiction which requires Road stamp, then yes. The addition of baffles could be considered as a minor alteration since the pressure boundary is not altered 



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: 'Ali Bhatti' via Materials & Welding <materials-welding@googlegroups.com>
Date: 01/01/2017 22:29 (GMT+02:00)
To: materials-welding@googlegroups.com
Subject: [MW:25859] R-stamp

Dear Experts

We have one  Vessel   to fix baffle plates . Vessel is under service since 9 years. Shell thickness is 38 mm and baffles plates thickness will be 7mm. My question are:
1. Is R-stamp required or not?  2. Is local PWHT required or not?
Please share / send me answer with reference of codes

Thanks and Best Regards

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/EEE7D9CD-935A-43E5-8101-8668CA4B4A9C%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...