Dear sir,
I have 1" s.s. pipe having thkness of 4.1mm. We have used x ray quality with D4 size film. We have shown the client, required IQI as per sec V.
But client wants 2% sensitivity as per specification.
Sensitivity= min thk of visible wire/ thk of base metal*100
In our case, sensitivity= 0.20/4.1*100.
So, it will come as 4.84 % .
So, how we will get 2% sensitivity.
Regards
Prasad
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/558a47dc-140a-4d01-9b43-f3be058368a5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production
Hi David, There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment