Dear Experts
We have one Vessel to fix baffle plates . Vessel is under service since 9 years. Shell thickness is 38 mm and baffles plates thickness will be 7mm. My question are:
1. Is R-stamp required or not? 2. Is local PWHT required or not?
Please share / send me answer with reference of codes
Thanks and Best Regards
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/EEE7D9CD-935A-43E5-8101-8668CA4B4A9C%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:34832] Inquiry about Single Bevel with Back Grinding
Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...