RE: [MW:25497] Requirement For Shoe Support Pad

It is not  indicated whether this line has been stress analysed. You can weld RF pad if analysis demands it.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pratish Kumar Anand
Sent: Wednesday, October 5, 2016 2:58 PM
To: Materials & Welding
Subject: [MW:25486] Requirement For Shoe Support Pad

 

Gentlemen s ,

 

I have 2" to 10" P1 material pipe for Thermic Fluid of design temperature is 250 degree cel. Drawing shows trunnion and shoe supports directly fully welded on the pipes of thickness range 2 to 10 mm . Pls suggest whether its acceptable or need to have a reinforcing pads which is not welded to pipe will be acceptable. 

 

 

 

Thanks in advance

 

Pratish

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f8ebb28b-de9b-4bd2-b909-adecf8cdd972%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...