Re: [MW:18969] Welder Repair Percentage Calculation

also i want to add one more doubt. generally we are taking only NDT taken joints in calculation. if welder did 100 joints but RT requirement is only 10%. so we took 10 joint RT. and suppose we have 2 joint repair in those RT joints than %repair = 2/10 * 100 = 20 %. we do not calculate other 90 joints.

is it OK ?

regards,


On Sun, Oct 13, 2013 at 6:52 AM, Richard robes <mech.processes@gmail.com> wrote:
Dear Gents,

I have one doubt regarding welder repair percentage rate calculation.

For one of welder he have done weld in 10" and 6". For 10" his repair percentage is 3 and for 6" his percentage is 2. For project its mentioned repair percentage for no. of joints welded shall not be more than 5 Percentage.

So if we add up his repair percentages it comes up to 3+2 = 5, but if we add up total no. of joints ie 10" and 6 " and then take total percentage repair rate come only up to 1.3 Percentage. 

Please advice which is the regular practice in doing repair calculation, whether its like adding up individual dia repair percentage or total no. of joints repair percentage?

Regards
Richard

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...