Re: [MW:18965] Cryogenic plant (Nitrogen generating unit liquid & gas ) Process piping welding with normal ER 308l fillerwire

Dear Lalit:

It's all about brittle fracture at these low temperatures.
If your impact test specimen fails to meet lateral expansion requirements, chances are the respective WPS (or filler metal) may not produce welds with sufficient low temperature toughness for you. It is not recommended to use such WPS (or filler metal).

Regards
Ramin Kondori
Sr. QA/QC Engineer
SINOPEC

r.kondori@petroyada.com
+98-2123592322
+98-9132150320



On Tue, Oct 15, 2013 at 1:56 PM, LALIT VADADORIYA <lalit.vadadoriya@gmail.com> wrote:
Dear Sir,

What's problem happen in future?

(1) If wr are using   ER 308L filler wire without carring lateral expansion at -196 in ss 304l process piping in cryogenic (Nitrogen generating) plant  (Liquid/gas  fluid).

(2) If we are using both filler wire ER 308L with lateral expansion (0.38mm ) at -196 degree. & ER 308L without lateral expansion. how to segregate the joints in this case.

regards 

lalit

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...