Dear Brother , Check the % of Oxygen during Purging by OXYGEN MONITOR INSTRUMENT AVAILABLE.

On Wed, Oct 9, 2013 at 9:24 AM, smkabeer ahamed <sm_kabeerahamed@yahoo.co.in> wrote:


On Tuesday, 8 October 2013 11:51 AM, smkabeer ahamed <sm_kabeerahamed@yahoo.co.in> wrote:

Dear friends,

stainless steel welding ss304 to ss304 I have used TIG welding at groove
joint.I have used argon gas purity level 99.7 percent instead of
99.99percent .our client suspect weld joint get oxidized.Is this purity
level is accepted as per any code How we will check what percent of
oxidation available in joint.is any testing method is there.how we will
convince our client and get approval from him.kindly suggest as early as
possible

Regards,

S.M.KABEER AHAMED
CHIEF ENGINEER
QUEST INSPECTION AGENCY
BANGALORE-INDIA


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...