Tuesday, October 1, 2013

Re: [MW:18827] Option for E6010 in root welding

Dear,
if you want to use E 7018,Qualify the WPS as per Requirement. for E7010-P1 you can use as root pass welding,even you have the WPS E6010.becoz both in same grouping non essential variables,but required to revise the WPS.



On Tue, Oct 1, 2013 at 8:08 AM, Sam <onlyprivate2007@gmail.com> wrote:
dear sir thanks for your reply.

1) i mean can we use other electrodes like E7010-P1 or E7018 in pipeline root welding or any other ?
3) Why we use E7010 electrodes in filling/capping with combination of E6010 in root for same API 5L X42 or A106 Gr.B carbon steel pipeline, if E7010 is for alloy steel ?


On Mon, Sep 30, 2013 at 7:08 AM, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:
E6010 is used only for root weld in pipe line because during welding (cellulose electrodes) decomposes cellulose + water, generates carbon monoxide and Hydrogen, Hydrogen gas is poor electrical conductor and has a high ionization potential that causes the resistance of the arc opening to increase and the electrons emission to decrease, which result in a higher arc voltage and more penetrating arc   


On Sun, Sep 29, 2013 at 4:07 PM, Srini Vasan <srinicwi@gmail.com> wrote:

E 6010 is most suitable for deeply penetrarion,also it reduces slag inclusion.but if we use E 7018 we cant achieve good penetration.E 6010 electrodes mostly utilized in pipelines,for deep penetration and good characteristics.

On 29 Sep 2013 13:26, "Octane Mac" <octane.mac@gmail.com> wrote:
1) Question is not clear. What do you mean by option?
2) E7018 arc is not deeply penetrating like of E6010
3) E7010-A1 contains 0.5% Mo unlike E6010. There isn't any similar E7010 like E6010. SFA 5.5 deals with alloyed steels and 5.1 with carbon steel.

Octane


On Sun, Sep 29, 2013 at 9:57 AM, Sam <onlyprivate2007@gmail.com> wrote:
Dear experts,

1) i want to learn that is there any option of E6010 in root welding of pipe by SMAW available ? i do know that same E6010 used for API 5L grade B, 42 and upto grade 60 also. 

2) If we use E7018 in root (when it suits UTS of base metal) , what is the main problem ? is it only about slag in inside face  and penetration ?

3) Why E6010 is AWS SFA 5.1 and same E7010 is AWS SFA 5.5 (both looks same except UTS) ?

please answer in details.

Regards,
sam.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
With Best & Regards

N.Srinivas,
Welding Inspector,
Al Suwaiket Industrial Support Services,
0561198050,0537812787
Al-Khobar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...