In addition to below mail, Please also consider below details.
Process Service : Polyethylene Powder
Design Temp.: 130° C
Design Pressure: 38 Kg/Cm2
Regds/Jignesh
---------- Forwarded message ----------
From: Jignesh Desai <jignesh.desai.met@gmail.com>
Date: Tue, Oct 8, 2013 at 11:02 AM
Subject: Welding of Duplex SS (A 790 Grade S31803) P. No. - 10H to SS 304, P No. 8
To: materials-welding@googlegroups.com
We have carried out PQR (ASME Sec IX) for Welding of Duplex SS (A 790 Grade S31803) P. No. - 10H to SS 304, P No. 8 by GTAW filler wire ER 309L. This filler wire is adopted as per API 582 (Table A-3) and also after client approval on PWPS.
From: Jignesh Desai <jignesh.desai.met@gmail.com>
Date: Tue, Oct 8, 2013 at 11:02 AM
Subject: Welding of Duplex SS (A 790 Grade S31803) P. No. - 10H to SS 304, P No. 8
To: materials-welding@googlegroups.com
We have carried out PQR (ASME Sec IX) for Welding of Duplex SS (A 790 Grade S31803) P. No. - 10H to SS 304, P No. 8 by GTAW filler wire ER 309L. This filler wire is adopted as per API 582 (Table A-3) and also after client approval on PWPS.
Now client is quoting that they have some bitter experience with ER 309L and insisting us to use GTAW filler wire ER 2209.
Does any one have any past experience / literature for Welding of Duplex SS (A 790 Grade S31803) P. No. - 10H to SS 304, P No. 8 by GTAW filler wire ER 309L
Your reply may possibly strengthen our case.
Regds/Jignesh
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment