Yes you can make SMAW with Backing, OR only GTAW or GTAW+SMAW


From: sumod s <sumod.sadhupuram@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tuesday, 16 April 2013, 18:15
Subject: [MW:17440] Invidual WPS from combined PQR

Dear,
 
I have a PQR for GTAW +SMAW. Can i make seperate WPS for GTAW and SMAW(with backing) from this PQR. (with in all limits of thickness)
 
Sumod
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...